MnOx-TiO2, CeO2-MnOx-TiO2 and V2O5-MnOx-TiO2 catalysts for low-temperature NH3-SCR were prepared by sol-gel method. The results showed that both cerium and vanadium prevented the transformation ofanatase TiO2 to the m...MnOx-TiO2, CeO2-MnOx-TiO2 and V2O5-MnOx-TiO2 catalysts for low-temperature NH3-SCR were prepared by sol-gel method. The results showed that both cerium and vanadium prevented the transformation ofanatase TiO2 to the mille phase. The addition of vanadium oxide induced the segregation of crystalline Mn2O3, which contributed little to low-temperature SCR and ammonia oxidation, from the MnOx-TiO2 solid solutions. However, the selectivity of the V-containing catalyst was almost 100% due to the decreased ammonia consumption and enhanced adsorption capacity of ammonia on Bronsted acid sites at relatively high temperatures. The electron-donating effect of cerium reduced the Mn^4+/Mn^3- ratio to some extent, resulting in a decreased activity for ammonia oxidation. This, in combination with the enhanced ammonia adsorption capacity by Ce^n+ as additional Lewis acid sites, endowed the Ce-doped catalyst a higher N2 selectivity than MnOx-TiO2 despite the slightly elevated light-offtemperamre for NO conversion.展开更多
The effects of atmospheres and precursors on MnOx/TiO2 catalysts were studied, which were prepared by the impregnation method and tested for their NOx conversion activity in ammonia selective catalytic reduction (NH3...The effects of atmospheres and precursors on MnOx/TiO2 catalysts were studied, which were prepared by the impregnation method and tested for their NOx conversion activity in ammonia selective catalytic reduction (NH3-SCR) reactions. Results showed that the manganese carbonate (MC) precursor caused mainly Mn2O3, while the manganese nitrate (MN) precursor resulted primarily in MnO2 and the manganese sulfate (MS) precursor was unchanged. The manganese acetate (MA) precursor leaded obtaining a mixture of Mn2O3 and Mn304. NOn conversion decreased in the following order: MA/TiO2 〉 MC/TiO2 〉 MN/TiO2 〉 MS/TiO2 〉 P25, with a calcination temperature of 773 K in air. Catalysts that were prepared by MA and calcined in oxygen performed strong interaction between Ti and Mn, while MnTiO3 was observed. Compared to the catalysts calcined in nitrogen, those calcined in oxygen had larger diameter and smaller surface area and pore. Catalysts that were prepared by MA and calcined in nitrogen tended to gain higher denitration rates than those in air, since they could be prepared with significant specific surface areas. NO., conversion decreased with calcination atmospheres: Nitrogen〉 Air〉 Oxygen. Meanwhile, amorphous Mn2O3 turned into crystalline Mn2O3, when the temperatures increased from 673 to 873 K.展开更多
A series of Ce-doped MnOx/TiO2 catalysts were prepared by impregnation method and used for catalytic oxidation of NO in the presence of excess O2. The sample with the Ce doping concentration of Ce/Mn=l/3 and calcined ...A series of Ce-doped MnOx/TiO2 catalysts were prepared by impregnation method and used for catalytic oxidation of NO in the presence of excess O2. The sample with the Ce doping concentration of Ce/Mn=l/3 and calcined at 300 ℃ shows a superior activity for NO oxidation to NO2. On Ce(1)Mn(3)Ti catalyst, 58% NO conversion was obtained at 200 ℃ and 85% NO conversion at 250 ℃ with a GHSV of 41000 h-1, which was much higher than that over MnOx/TiO2 catalyst (48% at 250 ℃). Characterization results implied that the higher activity of Ce(1)Mn(3)Ti could be attributed to the enrichment of well-dispersed MnO2 on the surface and the abundance of Mn3+ and Zi3+ species. The addition of Ce into MnO2/TiO2 could improve oxygen storage capacity and facilitate oxygen mobility of the catalyst as shown by PL and ESR, so that its activity for NO oxidation could be enhanced. The effect of H2O and SO2 on the catalyst activity was also investigated.展开更多
The performance of Mn-W/TiO2 for selective catalytic reduction(SCR) of NOx with NH3 and its resistance to different concentrations of SO2 at various temperatures were investigated. The results show that WO3 increase...The performance of Mn-W/TiO2 for selective catalytic reduction(SCR) of NOx with NH3 and its resistance to different concentrations of SO2 at various temperatures were investigated. The results show that WO3 increased the active sites and enhanced the strength of acid, so it was an effective promoter of MnOJTiO2. The NOx conversion on Mn-W/TiO2 ranges from 80.3% to 99.6% between 100 ℃to 350℃ at GHSV=18900 h 1, while N2 product selectivity changes from 100% to 98.7%. In the presence of 0.01% SO2 and 6% H20, NOx conversion maintained 98.5% at 120℃. The influence of more than 0.01% SO2 on the activity of MnOx-WO3/TiO2 will disappear if the temperature rises above 250℃. By means of heating and sweeping with He, the activity of the catalysts can be recovered. At 300℃, NOx conversion yielded 99% with 0.07% SO2 and reached the level of commercial V-W/TiO2 catalysts. The Mn-W/TiO2 catalyst showed excellent performance for SCR of NOx with NH3 in a wider range of temperature with strong tolerance to SO2.展开更多
The catalytic activities of MnOx-WO3/TiO2 for selective catalytic reduction(SCR) of NO with NH3 were investigated in a wide range of temperature and reaction condition.It yielded a NOx conversion of 80.3%—99.6% and...The catalytic activities of MnOx-WO3/TiO2 for selective catalytic reduction(SCR) of NO with NH3 were investigated in a wide range of temperature and reaction condition.It yielded a NOx conversion of 80.3%—99.6% and a N2 product selectivity of 100%—98.7% during 100 °C to 350 °C at gas hourly space velocity(GHSV)=18900 h-1.In the presence of 0.01% SO2 and 6% H2O at 120 °C,the NOx conversion can maintain 98.5%.At 300 °C and with 0.07% SO2 in reactant stream,the NOx conversion stabilized at 99% as high as the commercial V-W/TiO2 catalyst's level.The steady-state kinetics study shows that O2 played a promoting role.In the presence of less than 1.5% O2,NOx conversion can increase sharply with the increase of O2 concentration.The reaction order was zero with respect to NH3 and first with respect to NO with excess O2 and H2O.The kinetics active energy(Ea) of Mn-W/TiO2 was calculated to be 6.24 kJ/mol according to the kinetic experiment at various temperatures,much lower than those of other catalysts reported in the literature.Mn-W/TiO2 is an excellent catalyst for SCR of NO with NH3 by now.展开更多
基金Project supported by 863 Project (2009AA06Z313,2010CB732304)
摘要MnOx-TiO2, CeO2-MnOx-TiO2 and V2O5-MnOx-TiO2 catalysts for low-temperature NH3-SCR were prepared by sol-gel method. The results showed that both cerium and vanadium prevented the transformation ofanatase TiO2 to the mille phase. The addition of vanadium oxide induced the segregation of crystalline Mn2O3, which contributed little to low-temperature SCR and ammonia oxidation, from the MnOx-TiO2 solid solutions. However, the selectivity of the V-containing catalyst was almost 100% due to the decreased ammonia consumption and enhanced adsorption capacity of ammonia on Bronsted acid sites at relatively high temperatures. The electron-donating effect of cerium reduced the Mn^4+/Mn^3- ratio to some extent, resulting in a decreased activity for ammonia oxidation. This, in combination with the enhanced ammonia adsorption capacity by Ce^n+ as additional Lewis acid sites, endowed the Ce-doped catalyst a higher N2 selectivity than MnOx-TiO2 despite the slightly elevated light-offtemperamre for NO conversion.
基金Funded by the National "Twelfth Five-Year" Plan for Science&Technology Support of China(No.2011BAE29B02))
摘要The effects of atmospheres and precursors on MnOx/TiO2 catalysts were studied, which were prepared by the impregnation method and tested for their NOx conversion activity in ammonia selective catalytic reduction (NH3-SCR) reactions. Results showed that the manganese carbonate (MC) precursor caused mainly Mn2O3, while the manganese nitrate (MN) precursor resulted primarily in MnO2 and the manganese sulfate (MS) precursor was unchanged. The manganese acetate (MA) precursor leaded obtaining a mixture of Mn2O3 and Mn304. NOn conversion decreased in the following order: MA/TiO2 〉 MC/TiO2 〉 MN/TiO2 〉 MS/TiO2 〉 P25, with a calcination temperature of 773 K in air. Catalysts that were prepared by MA and calcined in oxygen performed strong interaction between Ti and Mn, while MnTiO3 was observed. Compared to the catalysts calcined in nitrogen, those calcined in oxygen had larger diameter and smaller surface area and pore. Catalysts that were prepared by MA and calcined in nitrogen tended to gain higher denitration rates than those in air, since they could be prepared with significant specific surface areas. NO., conversion decreased with calcination atmospheres: Nitrogen〉 Air〉 Oxygen. Meanwhile, amorphous Mn2O3 turned into crystalline Mn2O3, when the temperatures increased from 673 to 873 K.
基金supported by the National Natural Science Foundation of China (Grant No. 51078185)
摘要A series of Ce-doped MnOx/TiO2 catalysts were prepared by impregnation method and used for catalytic oxidation of NO in the presence of excess O2. The sample with the Ce doping concentration of Ce/Mn=l/3 and calcined at 300 ℃ shows a superior activity for NO oxidation to NO2. On Ce(1)Mn(3)Ti catalyst, 58% NO conversion was obtained at 200 ℃ and 85% NO conversion at 250 ℃ with a GHSV of 41000 h-1, which was much higher than that over MnOx/TiO2 catalyst (48% at 250 ℃). Characterization results implied that the higher activity of Ce(1)Mn(3)Ti could be attributed to the enrichment of well-dispersed MnO2 on the surface and the abundance of Mn3+ and Zi3+ species. The addition of Ce into MnO2/TiO2 could improve oxygen storage capacity and facilitate oxygen mobility of the catalyst as shown by PL and ESR, so that its activity for NO oxidation could be enhanced. The effect of H2O and SO2 on the catalyst activity was also investigated.
基金supported by the National Natural Science Foundation of China(51306046,51166004,51376073)the Fundamental Research Funds for the Universities of Henan Province(NSFRF140204)~~
摘要研究了Mn-W/TiO2用于NH3选择性催化还原NOx体系的催化反应性能,探索了不同温度条件下该催化剂对抗不同SO2浓度的抗毒性能。结果显示WO3能够增加活性酸中心的数量和酸性,是MnOx/TiO2非常有效的助催化剂。在气体体积空速(gaseous hourly space velocity,GHSV)为18900h-1时100~350℃范围内,Mn-W/TiO2催化剂还原NOx的转化率高达80.3%~99.6%,N2选择性达100%~98.7%。当反应气中有0.01%SO2和6%H2O时,120℃NOx转化率可维持在98.5%,当SO2浓度超过0.01%时,则需将反应温度升高到250℃以上才可消除其干扰,而当SO2浓度高达0.07%时,300℃下转化率可长期维持在99%,达到了商用V-W/TiO2催化剂的水平。对于NH3选择性还原NOx体系Mn-W/TiO2显示了极好的催化性能,是目前抗SO2毒性最强的催化剂之一。试验发现,低温条件下,SO2对Mn-W/TiO2催化剂的影响是可逆的,随着反应温度的提高,活性将自然恢复。
摘要The performance of Mn-W/TiO2 for selective catalytic reduction(SCR) of NOx with NH3 and its resistance to different concentrations of SO2 at various temperatures were investigated. The results show that WO3 increased the active sites and enhanced the strength of acid, so it was an effective promoter of MnOJTiO2. The NOx conversion on Mn-W/TiO2 ranges from 80.3% to 99.6% between 100 ℃to 350℃ at GHSV=18900 h 1, while N2 product selectivity changes from 100% to 98.7%. In the presence of 0.01% SO2 and 6% H20, NOx conversion maintained 98.5% at 120℃. The influence of more than 0.01% SO2 on the activity of MnOx-WO3/TiO2 will disappear if the temperature rises above 250℃. By means of heating and sweeping with He, the activity of the catalysts can be recovered. At 300℃, NOx conversion yielded 99% with 0.07% SO2 and reached the level of commercial V-W/TiO2 catalysts. The Mn-W/TiO2 catalyst showed excellent performance for SCR of NOx with NH3 in a wider range of temperature with strong tolerance to SO2.
摘要The catalytic activities of MnOx-WO3/TiO2 for selective catalytic reduction(SCR) of NO with NH3 were investigated in a wide range of temperature and reaction condition.It yielded a NOx conversion of 80.3%—99.6% and a N2 product selectivity of 100%—98.7% during 100 °C to 350 °C at gas hourly space velocity(GHSV)=18900 h-1.In the presence of 0.01% SO2 and 6% H2O at 120 °C,the NOx conversion can maintain 98.5%.At 300 °C and with 0.07% SO2 in reactant stream,the NOx conversion stabilized at 99% as high as the commercial V-W/TiO2 catalyst's level.The steady-state kinetics study shows that O2 played a promoting role.In the presence of less than 1.5% O2,NOx conversion can increase sharply with the increase of O2 concentration.The reaction order was zero with respect to NH3 and first with respect to NO with excess O2 and H2O.The kinetics active energy(Ea) of Mn-W/TiO2 was calculated to be 6.24 kJ/mol according to the kinetic experiment at various temperatures,much lower than those of other catalysts reported in the literature.Mn-W/TiO2 is an excellent catalyst for SCR of NO with NH3 by now.