TiO2-SiO2 thin films have been prepared on slide glass substrates by sol-gel method, and the effect of SiO2 additive on photo-generated hydrophilicity of TiO2 thin film was investigated by measuring the contact angle ...TiO2-SiO2 thin films have been prepared on slide glass substrates by sol-gel method, and the effect of SiO2 additive on photo-generated hydrophilicity of TiO2 thin film was investigated by measuring the contact angle of water, the microstructure, the transmittance, the photocatalytic activity and the specific surface area . The results showed that 10mol% of SiO2 additive was the most effective for decreasing contact angle of water. The SiO2 additive of less than 30mol% has a suppressive effect on the crystal growth of anatase in calcinations, resulting in a large surface area. Consequently, the super-hydrophilicity was improved.展开更多
In order to improve the corrosion resistance and biocompatibility of NiTi surgical alloy, TiO2 and TiO2-SiO2 thin films were prepared by sol-gel method. The surface characteristics of the film, which include surface c...In order to improve the corrosion resistance and biocompatibility of NiTi surgical alloy, TiO2 and TiO2-SiO2 thin films were prepared by sol-gel method. The surface characteristics of the film, which include surface composition, microstructure and surface morphology, were studied by X-ray diffraction (XRD), atomic force microscopy (AFM) and X-ray photoelectron spectra (XPS), respectively. A scratching test was used to assess the interface adhesive strength between the film and substrate. The corrosion resistance of NiTi alloy coated with oxide films were studied by anodic polarization curves measurement in biological solution. Additionally, a preliminary study of the in vitro bioactivity of the films was conducted. The results indicated that TiO2 and TiO2-SiO2 (Ti/Si=4:1) films have higher electrochemical corrosion resistance and can be used as protective layers on NiTi alloy. In addition, TiO2-SiO2 composite films have better bioactivity than TiO2 film.展开更多
A series of catalysts were prepared by doping different loadings of CeO2 over TiO2-SiO2-WO3 and used for the selective catalytic reduction of NOx by NH3. The experimental results showed that the selective catalytic re...A series of catalysts were prepared by doping different loadings of CeO2 over TiO2-SiO2-WO3 and used for the selective catalytic reduction of NOx by NH3. The experimental results showed that the selective catalytic reduction(SCR) performance and SO2-resistant ability of TiO2-SiO2-WO3 were greatly enhanced by the introduction of cerium. The catalyst containing 10% CeO2 showed the highest NO conversion in a wide temperature range and good N2 selectivity with broad operation temperature window at the gas hourly space velocity(GHSV) of 30000 h–1, which was a very promising catalyst for NOx abatement from diesel engine exhaust. The catalysts were characterized by X-ray diffraction(XRD), scanning electron microscopy with energy dispersive X-ray spectroscopy(SEM-EDS), N2 adsorption-desorption(BET) and X-ray photoelectron spectroscopy(XPS). The characterization results showed that the bigger pore radius, higher surface atomic concentration and dispersion of Ce and the abundant adsorbed oxygen on the surface of catalyst contributed to the best NH3-SCR performance of CeO2/TiO2-SiO2-WO3 catalyst containing 10% CeO2.展开更多
Zn-doped TiO2 (Zn?TiO2) thin films were prepared by the sol?gel method on titanium substrates with heat treatment at different temperatures. The effects of heat treatment temperatures and Zn doping on the structure, p...Zn-doped TiO2 (Zn?TiO2) thin films were prepared by the sol?gel method on titanium substrates with heat treatment at different temperatures. The effects of heat treatment temperatures and Zn doping on the structure, photocathodic protection and photoelectrochemical properties of TiO2 thin films were investigated. It is indicated that the photoelectrical performance of the Zn?TiO2 films is enhanced with the addition of Zn element compared with the pure-TiO2 film and the largest decline by 897 mV in the electrode potential is achieved under 300 °C heat treatment. SEM?EDS analyses show that Zn element is unevenly distributed in Zn?TiO2 films; XRD patterns reveal that the grain size of Zn?TiO2 is smaller than that of pure-TiO2; FTIR results indicate that Zn - O bond forms on Zn?TiO2 surface. Ultraviolet visible absorption spectra prove that Zn?TiO2 shifts to visible light region.Mott?Shottky curves show that the flat-band potential of Zn?TiO2 is more negative and charge carrier density is bigger than that ofpure-TiO2, implying that under the synergy of the width of the space-charge layer, carrier density and flat-band potential, Zn?TiO2 with 300 °C heat treatment displays the best photocathodic protection performance.展开更多
A series of SO 2- 4/TiO 2 SiO 2 catalysts with different mass fractions of SiO 2 were prepared by sol gel method. The effect of adding SiO 2 on the crystal structure, specific surface area, oxygen adsorption, and acid...A series of SO 2- 4/TiO 2 SiO 2 catalysts with different mass fractions of SiO 2 were prepared by sol gel method. The effect of adding SiO 2 on the crystal structure, specific surface area, oxygen adsorption, and acidity of SO 2- 4/TiO 2 catalyst and its photocatalytic property for degradation of bromomethane was studied. The results showed that the specific surface area and amount of oxygen adsorption of catalyst were increased by addition of SiO 2, leading to the obvious increase on photocatalytic activity of SO 2- 4/TiO 2 SiO 2 catalysts and mineralization ratio of bromomethane. Comparing with SO 2- 4/TiO 2, the acidic strength and anti moisture ability of SO 2- 4/TiO 2 SiO 2 catalyst were decreased.展开更多
ZrO2/TiO2 composite photocatalytic film was produced on the pure titanium substrate using in-situ Zr(OH)4 colloidal particle by the micro-arc oxidation technique and characterized by scanning electron microscope (...ZrO2/TiO2 composite photocatalytic film was produced on the pure titanium substrate using in-situ Zr(OH)4 colloidal particle by the micro-arc oxidation technique and characterized by scanning electron microscope (SEM), energy dispersive X-ray (EDX), X-ray diffraction (XRD) and ultraviolet-visible (UV-Vis) spectrophotometer. The composite film shows a lamellar and porous structure which consists of anatase, futile and ZrO2 phases. The optical absorption edge of film is shifted to longer wavelength when ZrO2 is introduced to TiO2. Furthermore, the photocatalytic reaction rate constants of degradation of rhodamine B solution with ZrO2/TiO2 composite film and pure TiO2 film under ultraviolet irradiation are measured as 0.0442 and 0.0186 h 1, respectively.展开更多
TiO2 films were deposited at room temperature by DC pulse magnetron sputtering system.The crystalline structures,morphological features and photocatalytic activity of TiO2 films were systematically investigated by X-r...TiO2 films were deposited at room temperature by DC pulse magnetron sputtering system.The crystalline structures,morphological features and photocatalytic activity of TiO2 films were systematically investigated by X-ray diffraction(XRD),atomic force microscopy(AFM) and ultraviolet spectrophotometer,respectively.The results indicated that working pressure was the key deposition parameter in?uencing the TiO2 film phase composition at room temperature,which directly affected its photocatalytic activity.With increasing working pressure,the target self-bias decreases monotonously.Therefore,low temperature TiO2 phase(anatase) could be deposited with high working pressure.The anatase TiO2 films deposited with 1.4 Pa working pressure displayed the highest photocatalytic activity by the decomposition of Methyl Orange solution,which the degradation rate reached the maximum(35%) after irradiation by ultraviolet light for 1 h.展开更多
本文利用纳米TiO2粉体,以聚乙烯吡咯烷(PVP)为分散剂和结构引导剂,以正硅酸乙酯(TEOS)为纳米SiO2前驱体,在纳米TiO2粉体表面包覆纳米SiO2,制备纳米TiO2-SiO2复合粒子。将纳米TiO2-SiO2复合粒子整理到棉织物上,并通过十六烷基三甲氧...本文利用纳米TiO2粉体,以聚乙烯吡咯烷(PVP)为分散剂和结构引导剂,以正硅酸乙酯(TEOS)为纳米SiO2前驱体,在纳米TiO2粉体表面包覆纳米SiO2,制备纳米TiO2-SiO2复合粒子。将纳米TiO2-SiO2复合粒子整理到棉织物上,并通过十六烷基三甲氧基硅烷(HDTMS)低表面能修饰后,得到抗紫外和超疏水复合功能棉织物。探究制备纳米TiO2-SiO2复合粒子的最佳工艺,并对复合粒子和处理后棉织物进行表征。结果表明,当PVP用量为0.025%,硅钛比例为2∶1,氨水用量为5 m L时,纳米SiO2包覆TiO2效果较好。处理棉织物的抗紫外指数(UPF)达115.42,紫外线UVA(320420 nm)透过率为3.35%,接触角为156.54°,滚动角为8°,具有优异的抗紫外、超疏水性能。此外,处理棉织物经过24 h紫外线照射后,接触角仍为152.73°,滚动角仍可达到9°,实现了耐紫外线稳定性。展开更多
基金Funded by Key Scientific and Technological Items of the Ministry of Education (No.99087) .
摘要TiO2-SiO2 thin films have been prepared on slide glass substrates by sol-gel method, and the effect of SiO2 additive on photo-generated hydrophilicity of TiO2 thin film was investigated by measuring the contact angle of water, the microstructure, the transmittance, the photocatalytic activity and the specific surface area . The results showed that 10mol% of SiO2 additive was the most effective for decreasing contact angle of water. The SiO2 additive of less than 30mol% has a suppressive effect on the crystal growth of anatase in calcinations, resulting in a large surface area. Consequently, the super-hydrophilicity was improved.
基金This work was supported by the National Natural Science Foundation of China(No.50081001)the Education Department Project of Liaoning Province(No.202073425).
摘要In order to improve the corrosion resistance and biocompatibility of NiTi surgical alloy, TiO2 and TiO2-SiO2 thin films were prepared by sol-gel method. The surface characteristics of the film, which include surface composition, microstructure and surface morphology, were studied by X-ray diffraction (XRD), atomic force microscopy (AFM) and X-ray photoelectron spectra (XPS), respectively. A scratching test was used to assess the interface adhesive strength between the film and substrate. The corrosion resistance of NiTi alloy coated with oxide films were studied by anodic polarization curves measurement in biological solution. Additionally, a preliminary study of the in vitro bioactivity of the films was conducted. The results indicated that TiO2 and TiO2-SiO2 (Ti/Si=4:1) films have higher electrochemical corrosion resistance and can be used as protective layers on NiTi alloy. In addition, TiO2-SiO2 composite films have better bioactivity than TiO2 film.
基金supported by the National Natural Science Foundation of China(21173153)the National High Technology Research and Development Program of China(863 project)(2013AA065304)
摘要A series of catalysts were prepared by doping different loadings of CeO2 over TiO2-SiO2-WO3 and used for the selective catalytic reduction of NOx by NH3. The experimental results showed that the selective catalytic reduction(SCR) performance and SO2-resistant ability of TiO2-SiO2-WO3 were greatly enhanced by the introduction of cerium. The catalyst containing 10% CeO2 showed the highest NO conversion in a wide temperature range and good N2 selectivity with broad operation temperature window at the gas hourly space velocity(GHSV) of 30000 h–1, which was a very promising catalyst for NOx abatement from diesel engine exhaust. The catalysts were characterized by X-ray diffraction(XRD), scanning electron microscopy with energy dispersive X-ray spectroscopy(SEM-EDS), N2 adsorption-desorption(BET) and X-ray photoelectron spectroscopy(XPS). The characterization results showed that the bigger pore radius, higher surface atomic concentration and dispersion of Ce and the abundant adsorbed oxygen on the surface of catalyst contributed to the best NH3-SCR performance of CeO2/TiO2-SiO2-WO3 catalyst containing 10% CeO2.
基金Project(cstc2011jj A50008)supported by the Natural Science Foundation of Chongqing,ChinaProject(14ZB0025)supported by Education Department of Sichuan Province,China
摘要Zn-doped TiO2 (Zn?TiO2) thin films were prepared by the sol?gel method on titanium substrates with heat treatment at different temperatures. The effects of heat treatment temperatures and Zn doping on the structure, photocathodic protection and photoelectrochemical properties of TiO2 thin films were investigated. It is indicated that the photoelectrical performance of the Zn?TiO2 films is enhanced with the addition of Zn element compared with the pure-TiO2 film and the largest decline by 897 mV in the electrode potential is achieved under 300 °C heat treatment. SEM?EDS analyses show that Zn element is unevenly distributed in Zn?TiO2 films; XRD patterns reveal that the grain size of Zn?TiO2 is smaller than that of pure-TiO2; FTIR results indicate that Zn - O bond forms on Zn?TiO2 surface. Ultraviolet visible absorption spectra prove that Zn?TiO2 shifts to visible light region.Mott?Shottky curves show that the flat-band potential of Zn?TiO2 is more negative and charge carrier density is bigger than that ofpure-TiO2, implying that under the synergy of the width of the space-charge layer, carrier density and flat-band potential, Zn?TiO2 with 300 °C heat treatment displays the best photocathodic protection performance.
摘要A series of SO 2- 4/TiO 2 SiO 2 catalysts with different mass fractions of SiO 2 were prepared by sol gel method. The effect of adding SiO 2 on the crystal structure, specific surface area, oxygen adsorption, and acidity of SO 2- 4/TiO 2 catalyst and its photocatalytic property for degradation of bromomethane was studied. The results showed that the specific surface area and amount of oxygen adsorption of catalyst were increased by addition of SiO 2, leading to the obvious increase on photocatalytic activity of SO 2- 4/TiO 2 SiO 2 catalysts and mineralization ratio of bromomethane. Comparing with SO 2- 4/TiO 2, the acidic strength and anti moisture ability of SO 2- 4/TiO 2 SiO 2 catalyst were decreased.
基金Project(gf200901002)supported by the Open Research Fund of National Defense Key Disciplines Laboratory of Light Alloy Processing Science and Technology of Nanchang Hangkong University,China
摘要ZrO2/TiO2 composite photocatalytic film was produced on the pure titanium substrate using in-situ Zr(OH)4 colloidal particle by the micro-arc oxidation technique and characterized by scanning electron microscope (SEM), energy dispersive X-ray (EDX), X-ray diffraction (XRD) and ultraviolet-visible (UV-Vis) spectrophotometer. The composite film shows a lamellar and porous structure which consists of anatase, futile and ZrO2 phases. The optical absorption edge of film is shifted to longer wavelength when ZrO2 is introduced to TiO2. Furthermore, the photocatalytic reaction rate constants of degradation of rhodamine B solution with ZrO2/TiO2 composite film and pure TiO2 film under ultraviolet irradiation are measured as 0.0442 and 0.0186 h 1, respectively.
基金supported by the Dalian Foundation for Development of Science and Technology (No.2006A13GX029)
摘要TiO2 films were deposited at room temperature by DC pulse magnetron sputtering system.The crystalline structures,morphological features and photocatalytic activity of TiO2 films were systematically investigated by X-ray diffraction(XRD),atomic force microscopy(AFM) and ultraviolet spectrophotometer,respectively.The results indicated that working pressure was the key deposition parameter in?uencing the TiO2 film phase composition at room temperature,which directly affected its photocatalytic activity.With increasing working pressure,the target self-bias decreases monotonously.Therefore,low temperature TiO2 phase(anatase) could be deposited with high working pressure.The anatase TiO2 films deposited with 1.4 Pa working pressure displayed the highest photocatalytic activity by the decomposition of Methyl Orange solution,which the degradation rate reached the maximum(35%) after irradiation by ultraviolet light for 1 h.
摘要本文利用纳米TiO2粉体,以聚乙烯吡咯烷(PVP)为分散剂和结构引导剂,以正硅酸乙酯(TEOS)为纳米SiO2前驱体,在纳米TiO2粉体表面包覆纳米SiO2,制备纳米TiO2-SiO2复合粒子。将纳米TiO2-SiO2复合粒子整理到棉织物上,并通过十六烷基三甲氧基硅烷(HDTMS)低表面能修饰后,得到抗紫外和超疏水复合功能棉织物。探究制备纳米TiO2-SiO2复合粒子的最佳工艺,并对复合粒子和处理后棉织物进行表征。结果表明,当PVP用量为0.025%,硅钛比例为2∶1,氨水用量为5 m L时,纳米SiO2包覆TiO2效果较好。处理棉织物的抗紫外指数(UPF)达115.42,紫外线UVA(320420 nm)透过率为3.35%,接触角为156.54°,滚动角为8°,具有优异的抗紫外、超疏水性能。此外,处理棉织物经过24 h紫外线照射后,接触角仍为152.73°,滚动角仍可达到9°,实现了耐紫外线稳定性。